| Impact Value | Testing Temperature | |||
| as welded | ||||
| 130 J (96 ft-lb) | 20 degC (68 degF) | |||
| 65 J (48 ft-lb) | -60 degC (-76 degF) | |||
| Elongation | Tensile Strength | Yield Strength |
| 30 % | 610 MPa (88.5 ksi) | 500 MPa (72.5 ksi) |
| Wire Electrode | SFA/AWS A5.9 : ER309LMo (mod) EN ISO 14343-A : W 23 12 2 L |
| Grade | VL 309 MoL (I1) |
| Society | DNV-GL |
| Approvals are based on factory location. Please contact ESAB for more information. |
| Alloy Type | Austenitic (with approx. 8% ferrite) "309LMo", 22 % Cr - 15 % Ni - 3 % Mo - Low C |
| Wire Composition | ||||||||||||||
| C | Cr | Mn | Mo | Ni | Si | |||||||||
| 0.01 % | 21.4 % | 1.5 % | 2.5 % | 14.6 % | 0.4 % | |||||||||
| Диаметр прутка,мм | 2.4 |
|---|
| Диаметр прутка,мм | 2.0 |
|---|